MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Haynes Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled
Categories: Metal; Superalloy; Iron Base

Material Notes: Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and is readily fabricated. Current applications include aircraft, including tailpipes and tailcones, afterburner parts, exhaust manifolds, combustion chambers, turbine blades, buckets and nozzles. Excellent service for high temperature bolts.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: AMS 5794, UNS R30155, AMS 5532, AMS 5768, AMS 5769, AMS 5795
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 159Converted from Rockwell B hardness.
Hardness, Knoop 176Converted from Rockwell B hardness.
Hardness, Rockwell B 92
Hardness, Vickers 201Converted from Rockwell B hardness.
Tensile Strength, Ultimate 814 MPa
 18.0 MPa
@Temperature 1288 °C
 23.0 MPa
@Temperature 1260 °C
 33.0 MPa
@Temperature 1204 °C
 48.0 MPa
@Temperature 1149 °C
 90.0 MPa
@Temperature 1093 °C
 170 MPa
@Temperature 982 °C
 268 MPa
@Temperature 871 °C
 403 MPa
@Temperature 760 °C
 507 MPa
@Temperature 649 °C
 647 MPa
@Temperature 538 °C
 676 MPa
@Temperature 427 °C
Tensile Strength, Yield 400 MPa
@Strain 0.2 %
 21.0 MPa
@Strain 0.2 %,
Temperature 1204 °C
 30.0 MPa
@Strain 0.2 %,
Temperature 1149 °C
 58.0 MPa
@Strain 0.2 %,
Temperature 1093 °C
 117 MPa
@Strain 0.2 %,
Temperature 982 °C
 207 MPa
@Strain 0.2 %,
Temperature 871 °C
 247 MPa
@Strain 0.2 %,
Temperature 760 °C
 259 MPa
@Strain 0.2 %,
Temperature 649 °C
 274 MPa
@Strain 0.2 %,
Temperature 538 °C
 292 MPa
@Strain 0.2 %,
Temperature 427 °C
Elongation at Break 49 %in 50.8 mm
 7.0 %
@Temperature 1288 °C
in 50.8 mm
 12 %
@Temperature 760 °C
in 50.8 mm
 15 %
@Temperature 871 °C
in 50.8 mm
 19 %
@Temperature 1260 °C
in 50.8 mm
 28 %
@Temperature 649 °C
in 50.8 mm
 29 %
@Temperature 1204 °C
in 50.8 mm
 36 %
@Temperature 1149 °C
in 50.8 mm
 38 %
@Temperature 1093 °C
in 50.8 mm
 51 %
@Temperature 982 °C
in 50.8 mm
 54 %
@Temperature 427 °C
in 50.8 mm
 54 %
@Temperature 538 °C
in 50.8 mm
Modulus of Elasticity 200 GPa
 124 GPa
@Temperature 871 °C
 152 GPa
@Temperature 649 °C
 152 GPa
@Temperature 760 °C
 165 GPa
@Temperature 427 °C
 172 GPa
@Temperature 538 °C
Poissons Ratio 0.298RT
 0.315
@Temperature 426 °C
 0.319
@Temperature -78.0 °C
 0.325
@Temperature 650 °C
 0.339
@Temperature 816 °C
Shear Modulus 77.0 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000930 ohm-cm
@Temperature 22.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.3 µm/m-°C
@Temperature 23.0 - 300 °C
 15.6 µm/m-°C
@Temperature 23.0 - 400 °C
 16.0 µm/m-°C
@Temperature 23.0 - 500 °C
 16.7 µm/m-°C
@Temperature 23.0 - 600 °C
 17.2 µm/m-°C
@Temperature 23.0 - 700 °C
 17.5 µm/m-°C
@Temperature 23.0 - 800 °C
 17.8 µm/m-°C
@Temperature 23.0 - 1000 °C
 17.8 µm/m-°C
@Temperature 23.0 - 900 °C
 18.4 µm/m-°C
@Temperature 23.0 - 1100 °C
Specific Heat Capacity 0.435 J/g-°C
@Temperature >=100 °C
Thermal Conductivity 15.9 W/m-K
@Temperature 300 °C
 17.3 W/m-K
@Temperature 400 °C
 18.6 W/m-K
@Temperature 500 °C
 20.0 W/m-K
@Temperature 600 °C
 20.0 W/m-K
@Temperature 200 °C
Melting Point 1288 - 1354 °C
Solidus 1288 °C
Liquidus 1354 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.88
@Temperature 1090 °C
Oxidized
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.080 - 0.16 %
Cb + Ta 0.75 - 1.25 %
Chromium, Cr 20 - 22.5 %
Cobalt, Co 18.5 - 21 %
Iron, Fe 33 %As remainder
Manganese, Mn 1.0 - 2.0 %
Molybdenum, Mo 2.5 - 3.5 %
Nickel, Ni 19 - 21 %
Nitrogen, N 0.10 - 0.20 %
Silicon, Si <= 1.0 %
Tungsten, W 2.0 - 3.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Haynes R-41 alloy, 0.635 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled
Haynes HR-160® alloy, annealed plate
Haynes 617 Nickel Alloy Plate
Haynes 556® alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened

NHAMAE / 16795

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.