MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® PTFE 660 PTFE + 60% bronze
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes: The high filler content results in significantly improved compressive strength and dimensional stability. This grade is not recommended for completely non-lubricated applications but is suitable for use with partially lubricating fluids such as hydraulic oil. The chemical resistance of the material is heavily restricted by the filler.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.85 g/ccDIN EN ISO 1183-1
Deformation 9.0 %
@Pressure 13.7 MPa,
Time 86400 sec
ASTM D 621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65DIN EN ISO 868
Ball Indentation Hardness 40.0 MPaDIN ISO 2039-1
Tensile Strength, Yield 15.0 MPaDIN EN ISO 527
Elongation at Break 125 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 1.30 GPaDIN EN ISO 527
Compressive Strength 12.0 MPa
@Strain 1 %
ASTM D 695
Charpy Impact, Notched 13.0 kJ/m²ISO 179-1/1eU
Coefficient of Friction 0.13pv = 0.7 N/mm2 · m/s; ASTM D3702
Coefficient of Friction, Static 0.10ASTM D3702
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+8 ohmDIN IEC 60023
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°C
@Temperature 23.0 - 95.0 °C
ASTM D 696
Thermal Conductivity 0.700 W/m-KDIN 52612-1
Melting Point 327 °C
Maximum Service Temperature, Air 260 °Clong term
Minimum Service Temperature, Air -200 °C
 
Descriptive Properties
Colorbronze

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP078 / 250576

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.