Key Features:- Ultra low viscosity
- Easily applied
- Unlimited working life at room temperature
- High temperature resistance properties
- Outstanding physical strength profile
- Superior electrical insulator
Product Description: Master Bond EP19HTLV is a one component very low viscosity epoxy for high performance impregnation, sealing and coating. It has unlimited working life at room temperature as it requires an elevated temperature cure at 250-300°F. The optimum curing schedule is 1 hour at 250°F followed by a post cure of 1-2 hours at 300-350°F. EP19HTLV bonds well to a wide variety of substrates such as ceramics, metals, composites, glass and many plastics. It combines outstanding physical strength properties with compelling electrical insulation properties. It has first rate chemical resistance to water, oils, fuels and many solvents. Its low viscosity allows for easy device temperature range extends from -60°F to +400°F allowing it to be used in a variety of applications requiring higher temperature resistance. It combines exceptionally low viscosity, impressive physical property profile and easy handling. This combination enables it to be a wonderful product for specialty aerospace, electronic and OEM type applications where porous surfaces, especially metals and ceramics, require impregnation or coating. It is most effective when applied under vacuum, although this is not mandatory.Product Advantages: - Ultra low viscosity; ideal for impregnation applications; sprayable or brushable
- Unlimited working life at room temperature
- Excellent physical strength properties
- Outstanding electrical insulation
- Superior heat resistance up to +400°F
- Good adhesion to a wide variety of substrates
Information provided by Master Bond Inc. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |