190 resin is suitable for use in hot melt adhesive and coating applications, as well as in carpet extrusion coating applications. It complies with Code of Federal Regulation 21 CFR Section 177.1520 subject to extraction limitations for specific end use applications. This polymer may be processed on conventional extrusion equipment. Additives: Applications: Adhesives & Sealants; Automotive Information provided by Celanese Corporation. |
hot melt coating and adhesive applications |