MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC SABIC® PP S3625 PP (Europe)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PPcompound S3625 is a 25% short glass fiber reinforced polypropylene copolymer compound for injection moulding applications. The compound is UV stabilized and the glass fibers are chemically coupled to the PP matrix. This compound combines a matt surface, good sound dampening and excellent scratch resistance with soft-touch haptics and is especially designed for aesthetical automotive interior applications. SABIC® PPcompound S3625 is a designated automotive grade. IMDS ID: 559182813

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccInjection molded sample ISO527-1A; ISO 1183
Filler Content 25 %SABIC method
Linear Mold Shrinkage 0.0040 cm/cmInjection molded plaque 65x65x3.2mm; SABIC method
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 35.0 MPaISO 527/1A
Tensile Strength, Yield 35.0 MPaISO 527/1A
Elongation at Break 7.0 %ISO 527/1A
Tensile Modulus 2900 MPaISO 527/1A
Flexural Modulus 2850 MPaISO 178/1A
Izod Impact, Notched (ISO) 35.0 kJ/m²N.B.: No Break; ISO 180/1A
 25.0 kJ/m²
@Temperature -20.0 °C
N.B.: No Break; ISO 180/1A
 30.0 kJ/m²
@Temperature 0.000 °C
N.B.: No Break; ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 81.0 µm/m-°C
@Temperature -30.0 - 100 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 111 °CISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11548 / 245015

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.