High strength, low alloy grade. May be substituted for more expensive normalized grades (A633) in certain applications. Normal uses are applications where notch toughness is an important design consideration. Information provided by Bethlehem Steel Corporation Data published in 1997. Bethlehem Steel in no longer in business. |