SABIC® PPcompound 8611A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of low density, good flow, high stiffness, and cold temperature ductility is required.
IMDS ID: 482236460Information provided by SABIC |