MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Molding M4825 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: ** NOTE: UL REGULATORY LISTING PENDING

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cmASTM D955
Spiral Flow 109.22 cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 84ASTM D2240
Tensile Strength, Yield 62.7 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 16 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 3290 MPaType I, 51 mm/min; ASTM D638
Flexural Strength 96.5 MPaASTM D790
Flexural Modulus 3240 MPaASTM D790
Izod Impact, Notched 53.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 63.9 °C
@Thickness 6.35 mm
Annealed; ASTM D648
 66.1 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
@Thickness 6.35 mm
Annealed; ASTM D648
 63.0 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 4.0 %
@Thickness 3.81 mm
ASTM D1003
Transmission, Visible 75 %
@Thickness 3.81 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 204 °C
 
Descriptive Properties
AppearanceClear/Transparent
FeaturesGeneral Purpose
 High Flow
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Product Description** NOTE: UL REGULATORY LISTING PENDING
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesGeneral Purpose

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Molding 6957 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid
Bayshore Vinyl Compounds BRC R409002 Molding Compound
Stratasys® RGD4825-DM Simulated Polypropylene Digital Material
Avient Novablend™ 6602 Polyvinyl Chloride, Rigid

PH0POL0567 / 145136

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.