MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: ARCEL is a high-performance, moldable foam resin consisting of 70% polystyrene (PS) and 30% polyethylene (PE). ARCEL provides toughness, flexibility and durability in a lightweight foam.

The strength and flexibility of ARCEL creates a resilient resin able to be molded into numerous complex and intricate forms. Its lightweight construction is resistant to puncture, flaking, tearing and breaking. In addition, packaging molded with ARCEL provides good cushioning and easy handling, while its lightweight properties help lower freight and other packaging costs.

ARCEL 730 is available in low-pentane (LV) grades for customers with strict pentane emission laws or high-density applications.

ARCEL 730 can be continuously or batch expanded using conventional EPS expansion equipment. Some minor material handling modifications may be required. For molded part densities below 1.5 pcf (24 g/l), double-pass expansion will be required to attain even lower bulk densities. ARCEL 730 has been expanded in continuous expanders ranging in size from 55 to 300 gallons as well as several sizes of batch expanders.

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0168 g/ccExpected from double pass expansion
 0.0210 g/ccExpected from batch expansion
 0.0216 g/ccExpected from single pass expansion
Particle Size 800 - 1700 µm98% range
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 48.0 psi1.5 pcf density
 75.0 psi2 pcf density
 100 psi2.4 pcf density
Compressive Strength 19.8 psi25% Deformation; 1.5 pcf density
 28.0 psi25% Deformation; 2.0 pcf density
 37.0 psi25% Deformation; 2.5 pcf density
Tear Strength 6.00 pli1.2 pcf density
 9.50 pli1.4 pcf density
 13.0 pli1.6 pcf density
 15.5 pli2.0 pcf density
 19.0 pli2.5 pcf density
Toughness 14.5 J1.2 pcf density
 16.5 J1.4 pcf density
 18.5 J1.6 pcf density
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0376 W/m-K0.032 g/cc density
 0.0381 W/m-K0.028 g/cc density
 0.0388 W/m-K0.024 g/cc density
 0.0395 W/m-K0.020 g/cc density
Insulation R Value 3.661.3 pcf density
 3.741.6 pcf density
 3.791.8 pcf density
 3.832.0 pcf density
Flame Spread 1.2 mm/min5.0 pcf density
 1.6 mm/min4.0 pcf density
 2.6 mm/min2.5 pcf density
 4.5 mm/minat 1.5 pcf density
 
Descriptive Properties
Average VOC Content10.5%(A low volatile grade is also available)
ColorWhite
Particle ShapeSpherical
StorageBelow 40°F (4°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding
BorsodChem ONGROSTYR F-I Expandable Polystyrene (EPS)
NOVA Chemicals ARCEL® 730B Expanded Polyethylene/Styrenic Polymer
NOVA Chemicals Expandable Polystyrene (EPS) 33MB Expandable Polystyrene Resin

PNOVA191 / 55092

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.