MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Covestro Desmodur® VP LS 2371 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Aliphatic polyisocyanate prepolymer based on isophorone diisocyanate. As a binder for elastic coatings and surface sealing compounds.

Properties / Applications: Desmodur® VP LS 2371 can be combined with latent hardeners such as Hardener® VP LS 2959 in the formulation of moisture-curing coatings. It can also be used with, for example, Hardener® DT and other special NH-functional co-reactants in the formulation of elastic coatings and surface sealing compounds for structural protection. On account of the polyether structure of this product, the resultant films are largely resistant to hydrolysis. However, if used outdoors, suitable light stabilizers must be added to counter the effects of sunlight.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccDIN EN ISO 2811
Viscosity 7300 - 12300 cPM014-ISO 3219/A.3
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 250 °CDIN EN 22 719
 
Descriptive Properties
Color40Hazen, M017-EN 1557
Content<2%Monomer, M106-ISO 10283
 3.4-4.0%NCO, M105-ISO 11909

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DESMODUR® TTG528 + MOCA Polyurethane, TDI- Ether
Covestro DESMODUR® TTX131 + MOCA, 85 A Polyurethane, TDI- PTMEG
Covestro DESMODUR® TTX142L + MOCA, 90 A Polyurethane, TDI- PTMEG
Covestro DESMODUR® TTX146 + MOCA, 90 A Polyurethane, TDI- PTMEG
Covestro DESMODUR® MTR31130 + BAYTEC® RT9265, 65 A Polyurethane, MDI- PTMEG

PCOVEST0671 / 202454

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.