MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient OnColor™ CC10075093WE Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: PG 75093.00 Pearl GD LDPE

Formula contains no wax or lubricants. Effective Date: 9/12/2005

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Carrier ResinLL/LDPE
FormsPellets
Generic MaterialTP, Unspecified
Generic NameThermoplastic, Unspecified (TP, Unspecified)
Let Down Ratio5%
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Usage2%
UsesColor Concentrates

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 1030 Low Density Polyethylene Extrusion/Injection Resin
Avient OnColor™ F Polyester, Thermoplastic
Toyobo Vylopet® EMC405A PET/PBT Blend
Polyplastics FR-PET® CN9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose
Polyplastics FR-PET® CN9015 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose

PH0POL0722 / 145291

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.