MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUPOL HF5157 PP+Rubber+MF, High Flow and Stiffness, High Impact
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced, Impact Modified

Material Notes: Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good Weatherability, Scratch Resistance

Application: Automotive Exterior (Slim wall Bumper Fascia)

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccASTM D792
Maximum Moisture Content 0.010Injection Molding
Linear Mold Shrinkage, Flow 0.0090 - 0.010 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 38 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 210 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 120 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Yield Strength 160 kg(f)/cm²
@Thickness 6.40 mm
10mm/min; ASTM D790
Flexural Modulus 19000 kg(f)/cm²
@Thickness 6.40 mm
10mm/min; ASTM D790
Izod Impact, Notched >= 6.20 kg-cm/cm
@Thickness 6.40 mm,
Temperature -10.0 °C
ASTM D256
 >= 48.0 kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 190 - 210 °CInjection Molding
Middle Barrel Temperature 200 - 230 °CInjection Molding
Front Barrel Temperature 200 - 230 °CInjection Molding
Nozzle Temperature 210 - 230 °CInjection Molding
Melt Temperature 200 - 230 °CInjection Molding
Mold Temperature 40.0 - 60.0 °CInjection Molding
Drying Temperature 70.0 - 80.0 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPaInjection Molding
Screw Speed 30 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOL HI5302RB PP+MF25%, High Impact
LG Chemical LUPOL HF5157Z PP+Rubber+MF, High Flow and Stiffness, High Impact
Entec Hypro™ PP-CP35/2 Impact Copolymer, 35 Melt Flow
Entec Hypro™ G PP-CP28NB Polypropylene

PLAY491 / 148501

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.