MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChenGuang Type B PTFE Vanished Glass-fabric
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Properties and applications: PTFE Varnished Glass-fabric possesses excellent electro-insulating properties, high temperature resistance, chemi-corrosion resistance, perfect non-sticky properties, as well as good mechanical strength. As an insulating material with high temperature resistance, it is used in some special electro-equipment and cable manufacture. As an outstanding non-sticky material, it is widely used in textile industry, food processing industry, petrochemical industry, wood processing industry as non-sticky conveyer belt etc., and also widely used in heat sealing of plastic packing bags as isolating layer.

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 100 MPaLongitudinal
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+11 ohm-cm
Surface Resistance >= 1.00e+12 ohm
Dielectric Constant 2.6 - 3.2
@Frequency 1e+6 Hz
Dielectric Loss Index <= 0.0050
@Frequency 1e+6 Hz
 
Descriptive Properties
Puncture voltage>0.3 KV0.08 mm, 50Hz
 >0.8 KV0.12 mm, 50Hz
 >1.3 KV0.23 mm, 50Hz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHENGU090 / 255689

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.