MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
LNP VALOX® EXCP0054 Polybutylene Terephthalate, 16% Carbon Fiber Reinforcement  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Carbon Black Filled

Material Notes:
  • Features: Solvent Resistant
  • Forms: Pellets
  • Processing Method: Injection Molding

Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 122 MPaType I, 5 mm/min; ASTM D638
Tensile Strength, Yield 122 MPaType I, 5 mm/min; ASTM D638
Elongation at Break 1.9 %Type I, 5 mm/min; ASTM D638
Elongation at Yield 1.9 %Type I, 5 mm/min; ASTM D638
Tensile Modulus 11.9 GPa5 mm/min; ASTM D638
Flexural Strength 197 MPa50.8 mm Span, 1 mm/min; ASTM D790
Flexural Modulus 11.7 GPa(50.8 mm Span) 1mm/min; ASTM D790
Izod Impact, Notched 0.320 J/cmASTM D256
Izod Impact, Unnotched 3.84 J/cmASTM D256
Falling Dart Impact 5.54 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1e+05ASTM D257
Static Decay <= 0.010 sec5000V to <50V; FTMS101B
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 202 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 238 - 254 °C
Middle Barrel Temperature 243 - 260 °C
Front Barrel Temperature 249 - 266 °C
Nozzle Temperature 243 - 260 °C
Melt Temperature 249 - 266 °C
Mold Temperature 65.6 - 87.8 °C
Drying Temperature 121 °C
Dry Time 3 - 12 hour
Moisture Content 0.020 %Suggested
Back Pressure 0.345 - 0.689 MPa
Clamp Pressure 41.0 - 83.0 MPa
Shot Size 40 - 80 %Suggested
Vent Depth 0.00250 - 0.00380 cm
Screw Speed 50 - 80 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with Carbon Black Filler
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
Orion Engineered Carbons PUREX® HS 55 Carbon Black
Orion Engineered Carbons ECORAX® 1720 Carbon Black
Orion Engineered Carbons CORAX® N 115 ASTM Carbon Black

PZLNP1578 / 51660

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.