MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Zircar Ceramics Z-MAG-B Non-RCF Blanket
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Mechanically needled silica magnesia fiber blanket provides much of the same performance found in ceramic fiber blanket but in a NON RCF composition.

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.54 g/cc
Filament Diameter 4.0 µm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 0.0350 MPaPerpendicular to Thickness; ASTM 686-76
Compression Set 78 %50% Compression, Parallel
 89 %30% Compression, Parallel
 96 %10% Compression, Parallel
 
Thermal PropertiesOriginal ValueComments
Insulation R Value 101
@Thickness 254 mm,
Temperature 1100 °C
Cold Face Temp, °C; 8 pcf density blanket
 114
@Thickness 203 mm,
Temperature 1100 °C
Cold Face Temp, °C; 8 pcf density blanket
 168
@Thickness 102 mm,
Temperature 1100 °C
Cold Face Temp, °C; 8 pcf density blanket
 243
@Thickness 50.8 mm,
Temperature 1100 °C
Cold Face Temp, °C; 8 pcf density blanket
 338
@Thickness 25.4 mm,
Temperature 1100 °C
Cold Face Temp, °C; 8 pcf density blanket
Melting Point 1500 °C
Maximum Service Temperature, Air 1260 °C
Shrinkage 1.7 %
@Temperature 1000 °C,
Time 90000 sec
8 pcf blanket (Perpendicular to Thickness)
 3.0 %
@Temperature 1260 °C,
Time 90000 sec
8 pcf blanket (Perpendicular to Thickness)
 
Component Elements PropertiesOriginal ValueComments
MgO 19 - 26 %
Other 0.00 - 4.0 %
SiO2 72 - 77 %
 
Descriptive Properties
ColorBluish White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mid-Mountain Materials CERMEX® PR2200SW Thermal Insulation Mat
Mid-Mountain Materials CERMEX® PR1800SW Low Biopersistence Thermal Insulation Paper
Magnesium Elektron Elektron® EQ21 Magnesium Casting Alloy, UNS M18330
Freudenberg S80 Silicone Elastomer (VMQ)
Ferro Aluminum Oxide Grinding Media P70

CZIR023 / 2831

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.