Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. Applications:Bynel® Series 4100 resins adhere to a variety of materials. They are most often used to adhere to EVOH, polyamide, PE, ionomers, and ethylene copolymers. Bynel® Series 4100 resins can be used in coextrusion processes including: blown filmcast film/sheetblow molding melt and solid phase thermoforming sheet and tubing In particular, Bynel® 41E687provides outstanding adhesion to ionomers, particularly sodium ionomers in blown film. A potential application in a barrier/ionomer structure is oil pouches or sachets. It is also useful in cook-in applications. Information provided by DuPont™ This former DuPont product line is now a Dow product line. |