MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SACO AEI PEXIDAN® SX-0650:CM603 Flame retardant compound for photovoltaic insulation & sheathing
Categories: Polymer; Thermoplastic

Material Notes: SX-0650:CM603 system is a low smoke, low fume, fire retardant silane crosslinkable compound which can be processed like a thermoplastic material at high output rates. The graft component, SX-0650, is mixed with the crosslinking catalyst masterbatch, catalyst CM603, generally in the ratio 95:5. Catalyst masterbatch CM601 can also be used for faster curing. The SX-0650 system has been developed to meet specification requirements TUV 2Pfg1169:2007, EN 50618:2014 and IEC 62930.

Information provided by SACO AEI Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 4.6Corrosivity of Gases; IEC 60754-2
Melt Flow 12 g/10 min
@Load 21.6 kg,
Temperature 150 °C
Storage Temperature 10.0 - 30.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 12.0 MPaIEC 60811-501
 13.8 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
after thermal ageing; IEC 60811-401
Elongation at Break 220 %IEC 60811-501
 187 %
@Treatment Temp. 150 °C,
Time 605000 sec
ageing behavior after; IEC 60811-401
Tensile Set 5.0 %
@Treatment Temp. 250 °C
Hot set after 45% elongation under load, 20N/cm2; IEC 60811-507
 
Electrical PropertiesOriginal ValueComments
Insulation Resistivity 12.0 Megaohm/1000 m
@Temperature 90.0 °C
BS EN 50395
 
Thermal PropertiesOriginal ValueComments
Oxygen Index >= 32 %BS ISO 4589-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CScrew water temperature
Zone 1 130 °C
Zone 2 140 °C
Zone 3 145 °C
Zone 4 150 °C
Die Temperature 160 °C
Head Temperature 160 °C
 
Descriptive Properties
Conductivity of Gases13 µS/cmIEC 60754-2
Halogen Acid Gas Evolution<0.5%IEC 60754-1
Thermal Endurance>20000 hrsat 120°C, BS EN 60216-1
Thermo-mechanical properties0.35Pressure test at high temperature 140°C, IEC 60811-508

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO069 / 265499

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.