MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC FLEX NORYL™ Resin WCA871A Polyphenylene Ether + TPE (PPE+TPE) (Americas)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyphenylene Ether/PPO

Material Notes: FLEX NORYL™ WCA871A resin is a flexible, non-reinforced extrudable blend of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE). This material contains non-halogenated flame retardant and performance capable of meeting UL VW-1 requirements, 105C end use temperature rating, and heat deformation performance as defined by UL 1581. FLEX NORYL WCA871A resin is intended for evaluation in wire insulation and cable jacket applications in light colors. It has a Shore A Hardness reading of 84 and exhibits superior thermal stability, very low water absorption, good electric properties, and low specific gravity. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.

Features: Flexible,Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Thin Wall,Non-Halogenated,Non-Chlorinated,Non-Brominated,Good Processability,Ductile

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8730s reading; ASTM D2240
Tensile Strength at Break 18.0 MPa50 mm/min; ASTM D638
 18.0 MPa50 mm/min; ISO 527
 27.0 MPaafter 7days @136°C; UL 1581
 30.0 MPaUL 1581
Elongation at Break 130 %50 mm/min; ISO 527
 140 %50 mm/min; ASTM D638
 200 %after 7days @136°C; UL 1581
 280 %UL 1581
Flexural Modulus 100 MPa12.5 mm/min, 100 mm span; ASTM D790
 100 MPa12.5 mm/min; ISO 178
Heat Distortion 20 %
@Load 0.250 kg,
Temperature 121 °C
UL 1581
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.40e+16 ohm-cmASTM D257
Dielectric Constant 2.6
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 28.0 kV/mm
@Thickness 1.50 mm
in oil; IEC 60243-1
Dissipation Factor 0.0028
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 105 °CUL temperature rating; UL 1581
Brittleness Temperature -40.0 °CASTM D746
Smoke Density 670.5mm plaque, Non-flame, Ds, max; ASTM E662
 1430.5mm plaque, Flame, Ds, max; ASTM E662
Oxygen Index 28 %ISO 4589
Glow Wire Ignition Temperature 825 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82051 / 289998

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.