MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® MP-1500 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments

Forms: Pellets

Processing Method: Extrusion; Injection Molding

Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C); Injection Rate: Fast

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 g/ccASTM D792
Linear Mold Shrinkage 0.016 in/inASTM D955
Melt Flow 1.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65ASTM D2240
Tensile Strength at Break 2100 psiASTM D412
Tensile Stress at Strain 800 psi
@Strain 300 %
ASTM D412
Elongation at Break 600 %ASTM D412
Tear Strength 38.6 kN/mDie B, 20 in/min; ASTM D624
 47.3 kN/mDie C, 20 in/min; ASTM D624
Compression Set 18 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 149 °FASTM D1525
Brittleness Temperature <= -76.0 °FISO 812
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 360 - 450 °F
Middle Barrel Temperature 370 - 460 °F
Front Barrel Temperature 380 - 470 °F
Nozzle Temperature 390 - 480 °F
Zone 1 360 - 450 °F
Zone 2 370 - 460 °F
Zone 3 380 - 470 °F
Zone 5 390 - 480 °F
Die Temperature 390 - 480 °F
Melt Temperature 390 - 480 °FProcessing Temperature
Mold Temperature 95.0 - 120 °F
Injection Pressure 200 - 800 psi
Back Pressure 25.0 - 100 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceClear/Transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Monprene® MP 1504 Thermoplastic Elastomer
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer
Teknor Apex Sarlink® 3490N Thermoplastic Elastomer
Teknor Apex Monprene® MP 1527 Thermoplastic Elastomer

PTEKNP634 / 129736

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.