MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ITW Densit® Ducorit® S8 Grout
Categories: Ceramic

Material Notes: Ducorit S8 is a strong structural grout primarily used in offshore wind turbine foundations. Its ability to be transferred pneumatically enables extremely fast material transfers from dock to vessel as well as ground-breaking installation speed.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 18.53 - 19.28 lb/galFresh grout
Grain Size <= 1000 µm
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 34.9 GPaStatic; ASTM C469
Flexural Strength 13.3 MPa40x40x160 mm prisms
Compressive Strength >= 90.0 MPa
@Temperature 20.0 °C
EN 12390-3
Poissons Ratio 0.20
 
Thermal PropertiesOriginal ValueComments
Shrinkage -0.0290 %Autogenous. Positive expansion; ASTM C1698
 
Component Elements PropertiesOriginal ValueComments
Free Water 14 - 15 %
 
Descriptive Properties
28 day Strength (MPa)11075 mm cubes
3 day Strength (MPa)83.775 mm cubes
Fatigue Factor0.95In water. DNV-OS_C502.
 1In air. DNV-OS_C502
Grout Thickness30 to 700 mm
Max. spread flow rate (mm)310ASTM C230 @ 20°C
Yield (l/kg)0.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWDE9070 / 239580

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.