MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay MIRAPOL® 550 P Surfactant
Categories: Fluid

Material Notes: Description: Mirapol 550 P can be used effectively in shampoos and conditioners at typical use levels of 0.5% (copolymer solids) to provide excellent lubricity, softeness light hair conditioning and combability improvements to hair without excessive build-up. Compatible with most surfactants systems, Mirapol 550 P could be used for transparent formulation for shower, bath gel, 2- in- 1 product, shampoo and rinse off conditionners. Mirapol 550 P is preserved with 0.1% of phenonip.

C.T.F.A. /I.N.C.I. Name: POLYQUATERNIUM – 7

CAS: 26590 – 05 – 6

Available in: Asia Pacific, Europe, Latin America and North America

Solubility: Soluble in water

Use level: 0.2-5%

Applications: MIRAPOL 550 P can be used effectively in shampoos and conditioners at typical use levels of 0.5% (copolymer solids) to provide excellent lubricity, softness, light hair conditioning and combability improvements to hair without excessive build-up. Compatible with most surfactants systems, MIRAPOL 550 P could be used for transparent formulation for shower, bath gel, 2- in-1 product, shampoo and rinse-off conditioners. MIRAPOL 550 P is preserved with 0.1% phenonip.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 6.5 - 7.5540MA3C1E
Viscosity 7500 - 15000 cP540MA3C52
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear viscous liquid540MA3C1F
Color<25Apha, 540MA3C1D
CompositionActives8.5-9.5%, 540MA3C09
 Residual acrylamide<5 ppm, 540MA3C53

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WRHOD264 / 137495

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.