MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Chrome-moly Steel; Tool Steel; Hot Work Steel

Material Notes: Chromium-molybdenum-tungsten-vanadium alloyed PM steel

Vanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications where wear resistance above that of an ORVAR 2M / AISI H13 is required. This material is available in limited sizes.

Vanadis 23 is characterized by:

  • High wear resistance (abrasive profile)
  • High compressive strength
  • Very good through-hardening properties
  • Good toughness
  • Very good dimensional stability on heat treatment
  • Very good temper resistance
Applications: Uddeholm Vanadis 23 is especially suitable for blanking and forming of thinner work materials where a mixed (abrasive–adhesive) or abrasive type of wear is encountered and where the risk for plastic deformation of the working surfaces of the tool is high, e.g.:Blanking of medium to high carbon steel
  • Blanking of harder materials such as hardened or cold-rolled strip steel
  • Plastics mould tooling subjected to abrasive wear condition
  • Plastics processing parts, e.g. feed screws, barrel liners, nozzles, screw tips, non-return check ring valves, pellitizer blades, granulator knives

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.287 lb/in³hardened and tempered
     0.281 lb/in³
    @Temperature 599 °C
    hardened and tempered
     0.283 lb/in³
    @Temperature 399 °C
    hardened and tempered
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Brinell 260Soft annealed (Delivery condition)
    Hardness, Rockwell C 57 - 66Tempering: 3 x 1 h at 1040°F
    Modulus of Elasticity 33000 ksi(hardened and tempered)
     27000 ksi
    @Temperature 599 °C
    hardened and tempered
     30000 ksi
    @Temperature 399 °C
    hardened and tempered
    Flexural Strength 5000 MPa(Fracture) @58HRC, Tempering: 3 x 1 h at 1040°F; Four-point bend
     5300 MPa(Fracture) @62HRC, Tempering: 3 x 1 h at 1040°F; Four-point bend
    Flexural Yield Strength 2700 MPa@58HRC, Tempering: 3 x 1 h at 1040°F; Four-point bend
     3500 MPa@64HRC, Tempering: 3 x 1 h at 1040°F; Four-point bend
    Impact Test 25.0 - 42.0 ft-lbunnotched; Tempering: 3 x 1 h at 1040°F
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 6.70 µin/in-°F
    @Temperature 399 °C
    hardened and tempered
     7.00 µin/in-°F
    @Temperature 599 °C
    hardened and tempered
    Specific Heat Capacity 0.100 BTU/lb-°Fhardened and tempered
     0.120 BTU/lb-°F
    @Temperature 399 °C
    hardened and tempered
     0.140 BTU/lb-°F
    @Temperature 599 °C
    hardened and tempered
    Thermal Conductivity 24.0 W/m-Khardened and tempered
     27.0 W/m-K
    @Temperature 599 °C
    hardened and tempered
     28.0 W/m-K
    @Temperature 399 °C
    hardened and tempered
    Shrinkage -0.130 - -0.0300 %Austenitizing and tempering
     
    Component Elements PropertiesOriginal ValueComments
    Carbon, C 1.28 %
    Chromium, Cr 4.2 %
    Iron, Fe 80.02 %As Balance
    Molybdenum, Mo 5.0 %
    Tungsten, W 6.4 %
    Vanadium, V 3.1 %
     
    Descriptive Properties
    Deflection, mm2.1@64HRC, Tempering: 3 x 1 h at 1040°F
     3.7@58HRC, Tempering: 3 x 1 h at 1040°F

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Assab Steels ASP 23 Cold Work Steel
    Crucible Steel CPM® 10V® (AISI A11) Tool Steel
    Bohler-Uddeholm UDDEHOLM VANADIS 6 Cold Work Tool Steel
    AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 315°C
    AISI Type M4 Molybdenum High Speed Tool Steel (UNS T11304)

    NBUCOR08 / 15477

    New MatWeb Services

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.