MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Hylar® Latex 932 PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Hylar® Latex 932 is a stabilized aqueous dispersion that contains approximately 22% by weight of a high molecular weight PVDF polymer (polyvinylidene fluoride) of medium crystallinity. The dispersion contains a non-ionic surfactant to stabilize against coagulation by conventional means.

Hylar® Latex 932 is useful for applications such as water-based coatings and fabric impregnation.

Applications: Coating Applications; Film

Features: Clean/High Purity; Crystalline; Good Strength; Good Toughness; Good Weather Resistance; High Gloss; High Molecular Weight; Low Odor; Radiation (Gamma) Resistant; UV Resistant

SAFETY

The dry polymer in Hylar® Latex 932 is stable at temperatures up to 315°C (600°F). When subjected to temperatures above 315°C (600°F) for extended periods of time, hydrogen fluoride (HF) begins to evolve. At temperatures above 371°C (700°F), HF evolution becomes rapid.

Thermal decomposition of the dry polymer in Hylar® Latex 932 can occur in melt processing operations as a result of excessive temperatures or in coating applications should the solvents be ignited, leading to fire. Thermal decomposition will generate HF, which is corrosive and causes burns on contact. It has an American Conference of Governmental Industrial Hygienists (ACGIH) Threshold Limit Value (TLV-TWA) of 3 ppm (2.5 mg/m3). In case of fire, use NIOSH approved self-contained breathing apparatus and skin protection to protect against volatile decomposition products such as HF and traces of toxic fluorocarbons.

In the event of thermal decomposition during melt processing operations, turn off the heat and evacuate the area until the area is cleared of HF. The dry polymer in Hylar® Latex 932 can be disposed of in an approved land fill. It should not be incinerated unless provision is made for absorption of HF.

SHELF LIFE

The practical limit shelf life of the material is 9 months from the production date, provided that the recommended storage conditions are maintained and the material remains free from foreign contamination during storage time.

STORAGE CONDITIONS (RECOMMENDED)

The material should remain un-opened in the original containers. The storage conditions should provide for protection from temperature extremes (<50°F and >75°F) and other conditions which may damage the containers in which the material is stored. Some settling may occur during storage; this should be reversible by agitation or rolling and should not affect the overall specifications as warranted.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 0.20 - 0.40 µm
pH 3.0 - 4.0
Viscosity 6.0 cP
 2900 - 3300 cP
@Shear Rate 100 1/s,
Temperature 232 °C
Melt; ASTM D3835
 
Thermal PropertiesOriginal ValueComments
Melting Point 156 - 160 °C
 
Descriptive Properties
AvailabilityEurope
 North America
ColorWhite
FormsLatex
ProcessingCoating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4258 / 280058

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.