MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC GELOY™ FXTW26SK ASA (Asia)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: ASA, Xtreme weatherability, high heat, with VisualFx.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Density 1.11 g/ccISO 1183
Water Absorption 0.50 %23°C/sat; ISO 62
Moisture Absorption 0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 12 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 13 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 36.0 MPa5 mm/min; ASTM D638
 36.0 MPa50 mm/min; ISO 527
 37.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 43.0 MPa5 mm/min; ASTM D638
 45.0 MPa50 mm/min; ISO 527
 46.0 MPa50 mm/min; ASTM D638
Elongation at Break 17 %50 mm/min; ASTM D638
 18 %5 mm/min; ASTM D638
 24 %50 mm/min; ISO 527
Elongation at Yield 2.5 %5 mm/min; ASTM D638
 2.7 %50 mm/min; ASTM D638
 2.8 %50 mm/min; ISO 527
Tensile Modulus 2450 MPa1mm/min; ISO 527
 2460 MPa5 mm/min; ASTM D638
Flexural Yield Strength 64.0 MPa2 mm/min; ISO 178
 74.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2500 MPa2 mm/min; ISO 178
 2570 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 140 J/mASTM D256
 23.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²80*10*4; ISO 180/1A
 2.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 8.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 18.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 83.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 84.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 94.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 94.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 84.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 95.0 °CRate B/50; ISO 306
 98.0 °CRate B/50; ASTM D1525
 99.0 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 220 - 255 °CInjection Molding
Zone 1 215 - 250 °C
Zone 2 220 - 255 °C
Zone 3 230 - 260 °C
Melt Temperature 240 - 270 °C
Mold Temperature 60.0 - 85.0 °C
Drying Temperature 85.0 - 90.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.040 %
Back Pressure 0.300 - 1.00 MPa
Shot Size 40 - 80 %
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10132 / 243599

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.