MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Trimay® Wear Plate TWP61 Complex-carbide Flux Cored Weld Wire & Electrode
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Description: TWP61 is a complex-carbide flux cored wire electrode used to protect equipment and parts from heavy wear in extreme temperatures. TWP61 has a unique composition that forms a tight crystalline matrix, and is able to deter heavy wear in temperatures up to 842oF (450oC).

Key Performance Characteristics: Heavy abrasion resistance, High heat resistance, Tight crystalline matrix,Good corrosion resistance

Applications: TWP61 can be overlain on carbon steel, manganese base materials and mild or alloy steels. The maximum recommended deposit thickness of TWP61 3/8” (9.53mm) in 2 - 3 layers. TWP61 is used for the installation of T157 wear plate and parts, as well as for hot wear applications such as burner tips, classifier cones and smokestacks.

Information provided by Trimay®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 60 - 64Electrodes
 63 - 65Wire
 
Component Elements PropertiesOriginal ValueComments
Boron, B <= 1.5 %
Carbon, C <= 5.0 %
Chromium, Cr <= 30 %
Iron, Fe <= 30 %
Manganese, Mn <= 2.0 %
Silicon, Si <= 2.0 %
Tungsten, W <= 1.5 %
Vanadium, V <= 1.0 %
 
Descriptive Properties
Available Sizes: Electrode3.25[mm]
 4[mm]
 5[mm]
Available Sizes: Wire1.1[mm], cored wire
 1.6[mm], cored wire
 2.4[mm], cored wire
 2.8[mm], cored wire
Packaging: Electrode3.25[mm] 4.5kg sleeves (4 sleeves=1 box)
 4[mm] 5kg sleeves (4 sleeves=1 box)
 5[mm] 5kg sleeves (4 sleeves=1 box)
Packaging: Wire1.1[mm], 15kg spools
 1.6[mm], 25kg spools
 2.4[mm], 25kg spools
 2.8[mm], 25kg spools

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wingate Alloys Winco-Tuf 36 High Strength Wear Plate
Wingate Alloys Champaloy Clad Overlay Wear Plate, Chrome Carbide Fusion Plate
Trimay® Wear Plate TWP56 Chromium-based Flux Cored Weld Wire & Electrode
Trimay® Wear Plate T170 Nickel-based Steel Overlay

NTRIM008 / 120822

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.