MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Dyneon™ PFA 6503PAZ Fluoroplastic Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: 3M™ Dyneon™ Fluoroplastic Powder PFA 6503PAZ is a fluorothermoplastic powder designed for use in thin film powder coatings. Typical applications include non-stick surfaces, chemical vessel and tank liners, electrical insulation and low friction applications.

    Features and Benefits:
  • Excellent electrostatics
  • Excellent non-stick performance
  • Outstanding flow and fluidization
  • Good stress crack resistance
  • Smooth surfaces
  • Good transparency
  • Non-wetting
  • Heat resistant to 260°C (500°F)
  • Low friction
  • Chemical resistance
  • Process target: powder coating
This product complies with 21 CFR 177.1550 FDA regulations

Information provided by the Dyneon division of 3M.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.15 g/ccASTM D792
Bulk Density 0.800 g/ccDIN 53466
Particle Size 30 µm
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 372 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
Tensile Strength at Break 30.0 MPaASTM D638
Elongation at Break 380 %ASTM D638
Flexural Modulus 550 MPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 308 °CASTM D4591
Maximum Service Temperature, Air 260 °C
Oxygen Index >= 95 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent, but thickness not quantified
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ THV 221AZ Fluoroplastic Agglomerate
3M Dyneon™ PFA 6503PBZ Fluoroplastic Powder
3M Dyneon™ ET 6210AZ Fluoroplastic Agglomerate

PDYL9958 / 129976

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.