- ASTM D 1056-07 2A2 grade material
- Fine cell – manufactured in blocks (buns)
- Approved source for Delphi SD2-207, paragraph 6.2
- Widely used, general purpose EPDM/CR/SBR blend
- ASTM D 6576-07 Type II, Grades B & C, condition soft-medium
Information provided by Armacell® |