MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Sandvik Sanicro 28 Bar Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Sanicro 28 is a high­alloy multi­purpose austenitic stainless steel for service in highly corrosive conditions. The grade is characterized by:
  • Very high corrosion resistance in strong acids
  • Very good resistance to stress corrosion cracking (SCC) and intergranular corrosion in various environments
  • High resistance to pitting and crevice corrosion
  • Good weldability

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 220
Tensile Strength, Ultimate 500 - 750 MPa
Tensile Strength, Yield 220 MPa
@Strain 0.2 %
Elongation at Break >= 35 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Chromium, Cr 27 %
Copper, Cu 1.0 %
Iron, Fe 34.8 %As Balance
Manganese, Mn <= 2.0 %
Molybdenum, Mo 3.5 %
Nickel, Ni 31 %
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.60 %
Sulfur, S <= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Sanicro 28 Seamless tube and pipe
Outokumpu 4565 High Performance Austenitic Stainless Steel
Sandvik 303-6RA11 Billet
Crucible Steel MCU Martensitic Steel
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel

NSANDV141 / 19035

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.