MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECAPET black Polyethylene terephthalate
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes:
  • very good chemical resistance
  • resistant to cleaning agents
  • excellent wear properties
  • excellent strength and stiffness
  • low moisture absorption
  • improved surface hardness
  • resistance against high energy radiation
Target Industries:
  • packaging and paper machinery
  • semiconductor technology
  • printing machines
  • mechanical engineering
  • pharmaceutical industry

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.38 g/cc
Moisture Absorption 0.500 %saturation; ASTM D 570
 0.0400 %
@Time 86400 sec
ASTM D 570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 93ASTM D 785
Hardness, Rockwell R 125ASTM D 785
Hardness, Shore D 85ASTM D 2240
Tensile Strength, Yield 10000 psiASTM D 638
Elongation at Break 50 %ASTM D 638
Elongation at Yield 4.0 %ASTM D 638
Modulus of Elasticity 485 ksiASTM D 638
Flexural Strength 16000 psiASTM D 790
Flexural Modulus 470000 psiASTM D 790
Compressive Yield Strength 14000 psi
@Strain 10 %
ASTM D 695
Compressive Strength 3600 psi
@Strain 1 %
ASTM D 695
Compressive Modulus 360000 psiASTM D 695
Izod Impact, Notched 0.530 ft-lb/inASTM D 256
Coefficient of Friction, Dynamic 0.25
@Pressure 0.276 MPa
50 fpm; ASTM D 3702
Coefficient of Friction, Static 0.19ASTM D 3702
K (wear) Factor 210 x 10-10 in³-min/ft-lb-hrAgainst Steel, 40 psi, 50 fpm; ASTM D 3702
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D 257
Dielectric Constant 3.4
@Frequency 60 Hz
ASTM D 150
Dielectric Strength 15.7 kV/mmASTM D 149
Dissipation Factor 0.020
@Frequency 60 Hz
ASTM D 150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 39.0 µin/in-°FASTM D 696
Specific Heat Capacity 0.280 BTU/lb-°F
Thermal Conductivity 2.01 BTU-in/hr-ft²-°F
Melting Point 490 °F
Maximum Service Temperature, Air 230 °FLong Term
 320 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 240 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 175 °FASTM D 648
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN8194 / 319122

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.