MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Sibur 15803-020 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: For production of films and film articles, including thin films, food contact grade films (including tight packing), general-purpose films, and bags.

Key Words: General Purpose Film Grade
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccGOST 15139
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
GOST 11645
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 11.7 MPa500 mm/min; GOST 11262
Tensile Strength, Yield 9.50 MPa500 mm/min; GOST 11262
Elongation at Break 600 %500 mm/min; GOST 11262
 
Descriptive Properties
Extractable Substances0.4 wt%GOST 26393
Odor and taste of aqueous extracts,1 pointGOST 22648
ProcessFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carmel Olefins Ipethene® 830 Low Density Polyethylene
Carmel Olefins Ipethene® 670 Low Density Polyethylene
Carmel Olefins Ipethene® 600 Low Density Polyethylene
Braskem PB 608 LDPE Injection Molding Polyethylene
Braskem PB 208 LDPE Injection Molding Polyethylene

PSIB004a / 159574

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.