This is a general purpose antiblock concentrate for use where freedom from blocking is important. Description/Features: - Diatomaceous Earth/ Silica
Market: Processing Method: Note: 1905 Antiblock PEC is acceptable for FDA applications depending on end use. Information provided by PolyOne Corporation. |