MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Network Polymers Nylon 6615 L
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description: Black Super Tough Nylon

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Water Absorption 1.2 %24 hours Immersion; ASTM D570
Linear Mold Shrinkage 0.016 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 119ASTM D785
Tensile Strength, Yield 7300 psiASTM D638
Elongation at Break 50 - 60 %ASTM D638
Flexural Strength 8000 psiASTM D790
Flexural Modulus 240000 psiASTM D790
Izod Impact, Notched 15.0 - 17.0 ft-lb/in1/8 in specimen; ASTM D256
 NB
@Temperature -40.0 °C
ASTM D256
Izod Impact, Unnotched 2.50 - 3.00 ft-lb/inASTM D256
 2.50 - 3.00 ft-lb/in
@Temperature -40.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 491 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 190 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Supreme Petrochem SP 256 Toughened Polystyrene
RTP Company RTP 100 GB 20 Z  Polypropylene (PP) Glass Bead 20% - FDA Type
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Lubrizol Isoplast® 301 Engineering Thermoplastic Polyurethane Resin
Chevron Phillips Marlex® SMX-360 Polypropylene Fiber Resin

PDIAM160 / 29998

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.