MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Evonik Vestodur® GF20-FR2 nf PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: ISO data as provided by the manufacturer, Creanova, Inc.

Glass fiber reinforced (20%), self-extinguishing PBT resin in accordance with UL 94 with non-migrating flame retardants and high rigidity.

This former Creanova product line is a part of Degussa AG as of 2001. This grade is not part of the current Degussa product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/cc
Water Absorption 0.00 %
Moisture Absorption at Equilibrium <= 0.50 %Humidity Absorption
Melt Flow 10 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 130 MPa
Elongation at Break 2.0 %
Modulus of Elasticity 7.50 GPa
Charpy Impact Unnotched 4.50 J/cm²
 4.50 J/cm²
@Temperature -30.0 °C
Charpy Impact, Notched 0.800 J/cm²
 0.700 J/cm²
@Temperature -30.0 °C
Tensile Impact Strength 55.0 kJ/m²
Tensile Creep Modulus, 1 hour 7500 MPa
Tensile Creep Modulus, 1000 hours 7000 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
Dielectric Constant 3.0
@Frequency 100 Hz
 4.0
@Frequency 1e+6 Hz
Dielectric Strength 27.0 kV/mm
Dissipation Factor 0.0030
@Frequency 100 Hz
 0.015
@Frequency 1e+6 Hz
Comparative Tracking Index 225 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear <= 50.0 µm/m-°C
@Temperature 20.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
Vicat Softening Point 210 °C50°C/hr/50 N
UL RTI, Electrical 140 °C
UL RTI, Mechanical with Impact 130 °C
UL RTI, Mechanical without Impact 130 °C
Flammability, UL94 V-0
@Thickness 1.60 mm
 V-0
@Thickness 3.20 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Pocan® B 4235 000000 PBT, 30% Glass Fiber
Shinkong Synthetic Fibers Shinite® D202G30 PBT, 30% Glass Filled, Fire Retardant
Evonik Vestodur® GF50 nf PBT
Envalior Pocan® B 3235 000000 PBT, 30% Glass Fiber
BASF Ultradur® S 4090 G6 30% Glass Filled PBT

PHUM15 / 47448

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.