MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Borealis FT6230 LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: FT6230 is an unmodified low density polyethylene based on the tubular technology for film extrusion and foam. This grade is developed for the production of packaging film with good optical properties for medium duty film applications.
Cas No. 9002-88-4
FT6230 contains: No additives

Applications:

  • Food packaging
  • Shrink film
  • Pouches
Typical characteristics:
  • Very good optical properties
  • Easy to extrude
  • Bubble stability

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccISO 1183-1
Melt Flow 2.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 400 %ISO 527-3
Film Elongation at Break, TD 600 %ISO 527-3
Tensile Modulus 190 MPaMD; ASTM D882
 210 MPaTD; ASTM D882
Coefficient of Friction 0.200film/film; ISO 8295
Elmendorf Tear Strength MD 235 gISO 6383-2
Elmendorf Tear Strength TD 255 gISO 6383-2
Dart Drop Test 100 gISO 7765-1
Film Tensile Strength at Break, MD 22.0 MPaISO 527-3
Film Tensile Strength at Break, TD 20.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 111 °CISO 11357-3
Vicat Softening Point 95.0 °C
@Load 1.02 kg
A50; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 8.00 %ASTM D1003
Gloss 70.0 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9781 / 323138

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.