MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Crosspolimeri EPIGUM EXP/53 PP
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Epigum: is the trade name of our halogen free thermoplastic materials.

Epigum ESH/P 831: is high performance thermoplastic PP modify material, thermally stable until 150°C, with continuous temperature rating 105°C. Suitable to use on medium voltage cable insulation. Readily recycled both in process and post consumer. The recipe contain metal deactivator

Certify: VDE0207-2 9YI2

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D792
Melt Flow 70 g/10 min
@Load 21.6 kg,
Temperature 220 °C
ISO 1133
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
Tensile Strength >= 16.0 MPaIEC 60811
Elongation at Break >= 500 %IEC 60811
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 125 °C
@Time 21600 sec
<10%, Penetration; IEC 60811
 
Processing PropertiesOriginal ValueComments
Zone 1 170 °C
Zone 2 180 °C
Zone 3 200 °C
Zone 4 215 °C
Die Temperature 230 °C
Head Temperature 225 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS045 / 294129

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.