MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Vinnapas® EF 575 Vinyl Acetate Ethylene
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product description: VINNAPAS® EF575 is an aqueous surfactant stabilized vinyl acetate-ethylene copolymer dispersion with a glass transition temperature (Tg) of 0 °C. It was developed as a versatile binder for use in a variety of applications including caulks, sealants, and mastics.

Properties:

  • Good adhesion to aluminum, galvanized and stainless steel.
  • Manufactured without the use of alkylphenol ethoxylate (APEO) surfactants or defoamers
  • Compatible with other binder chemistries
  • Can be formulated to pass numerous industry standards including ASTM C 834 and UL 181A/B.
  • Produced without the use of formaldehyde donors.
Application: Binder for caulks, sealants and mastics.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/cc
Solids Content 54 - 56 %
Particle Size 200 µm
pH 4.0 - 5.0
Brookfield Viscosity 200 - 850 cP#3 @ 60rpm
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 0.000 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9641 / 205170

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.