MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Machined Parts
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: High abrasion resistance, very low friction coefficient property, suitable for being applied to spin component of spin apparatus

Information provided by Daelim H&L

Key Words: PI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/ccASTM D792
Moisture Absorption at Equilibrium 0.90 %50% RH; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80 - 92ASTM D785
Tensile Strength, Ultimate 480 kg(f)/cm²
@Temperature 260 °C
ASTM D1708
 803 kg(f)/cm²
@Temperature 23.0 °C
ASTM D1708
Tensile Strength, Yield 601 kg(f)/cm²
@Strain 1 %
ASTM D95
Tensile Stress at Strain 1412 kg(f)/cm²
@Strain 10 %
ASTM D95
Elongation at Break 7.4 %
@Temperature 260 °C
ASTM D1708
 11.2 %
@Temperature 23.0 °C
ASTM D1708
Flexural Strength 64.7 MPa
@Temperature 260 °C
ASTM D790
 118.5 MPa
@Temperature 23.0 °C
ASTM D790
Flexural Modulus 26500 kg(f)/cm²
@Temperature 260 °C
ASTM D790
 38900 kg(f)/cm²
@Temperature 23.0 °C
ASTM D790
Compressive Modulus 2923.4 MPa
@Temperature 23.0 °C
ASTM D695
Izod Impact, Notched (ISO) 0.47088 J/cm²ASTM D256
Coefficient of Friction 0.20
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 - 1.00e+15 ohm-cm
@Temperature 23.0 °C
ASTM D257
Dissipation Factor 0.0104
@Frequency 1e+6 Hz,
Temperature 23.0 °C
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.70 µm/m-°C
@Temperature 23.0 - 260 °C
ASTM D696
Decomposition Temperature 616 °C
Oxygen Index 54.15 %ASTM D2863
 
Descriptive Properties
50% Weight Reduction Time (Minutes)240

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Machined Parts
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Machined Parts
Daelim H&L Plavis MS Aromatic Polyimide, 15% MoS2 Filled, Machined Parts
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Tubes

PDAEL003 / 82657

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.