Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses. TECAPEEK is a high-performance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique. Typical Applications: - Bearings and Bushings
- Down-hole instrumentation
- Wear Rings
- Ball Valve Seats
- Electrical Components
- Back-up and V-Rings
- Piston Rings and Rider Bands
Information provided by Ensinger Special Polymers, Inc. |
Metal Supermarkets is the World's largest supplier of small quantity metals. We feature any metal including Alloy Steel cut to size, unsurpasses service, and highest quality products. Referals from MatWeb receive a 2% discount!Ensinger Special Polymers, Inc. provides consistent, high quality compression molded stock shapes of engineering thermoplastics. Common shapes include rings, rods, plates, tubes, and discs. Large diameter rings up to 90" OD are available.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |