MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SAES Getters Lithium Niobate (LiNbO3)  (discontinued **)
Categories: Ceramic; Oxide

Material Notes: Optical-grade congruent lithium niobate crystal is a high quality, stable and reliable substrate for a wide range of applications, such as electro-optical modulators, acoustic-optical transducers, sensors and other waveguide-based advanced devices. Congruent composition is 48.56 mol% Li2O.

The well-established Ti-indiffusion and Proton Exchange technologies allow highly performance complex optical structures on SAES Getters congruent lithium niobate substrates.

Information provided by SAES Getters.

Key Words: LiNbO3 nominal
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.65 g/cc
 
Electrical PropertiesOriginal ValueComments
Curie Temperature 1140 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 1253 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 2.2025
@Wavelength 633 nm
ηe at 633 nm
 2.2865
@Wavelength 633 nm
ηo at 633 nm
Transmission, Visible 90 %
@Wavelength 320 - 5600 nm
IR Transmittance 90 %
@Wavelength 320 - 5600 nm
UV Transmittance 90 %
@Wavelength 320 - 5600 nm
 
Descriptive Properties
Coercive Field at RT20.6 kV/mm
Crystal StructureTrigonal
Point Group 3m

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lithium Niobate, LiNbO3
Lithium Borohydride, LiBH4
Lithium Borate, LiBO2
Lithium Azide, LiN3
Lithium Arsenate, Li3AsO4

CSAES00 / 1959

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.