MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) BLUESIL™ FLD 604V50 Dielectric Liquid
Categories: Fluid

Material Notes: Description: The following dielectric liquids are used to provide insulation and cooling in submerged transformers:
  • Mineral oils, which have the disadvantage of being inflammable,
  • Silicone oils, esters, etc.
BLUESIL FLD 604V50 is a dielectric liquid consisting of polydimethylsiloxane, whose purity has been checked especially for electrotechnical applications. BLUESIL FLD 604V50 is mainly used as an insulation and cooling medium for transformers and, more generally, for all medium tension equipment (switch boxes, chokes, capacitors, resistors, etc.) when environmental or fire safety problems arise, such as in public places, built-up areas, basements, proximity to water streams, etc. BLUESIL FLD 604V50 offers the following advantages:
  • Excellent dielectric properties
  • Excellent thermal stability
  • Remarkable chemical inertia and strength
  • Good heat transfer properties
  • Non-propagation of fire
  • Not dangerous for man or the environment

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/cc
Volatiles <= 0.50 %
@Temperature 150 °C,
Time 86400 sec
pH 6.7
Viscosity 14.2 cP
@Temperature 100 °C
 48 cP
@Temperature 25.0 °C
 83.8 cP
@Temperature 0.000 °C
 141 cP
@Temperature -20.0 °C
Kinematic Viscosity 50 cSt
@Temperature 25.0 °C
 85 cSt
@Temperature 0.000 °C
 140 cSt
@Temperature -20.0 °C
Kinematic Viscosity at 100°C (212°F) 16 cSt
@Temperature 100 °C
Surface Tension 20.7 dynes/cm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 9.10e+12 ohm-cm+5% of mineral oil; AFNOR NF C 27210
 1.50e+14 ohm-cm+2% of mineral oil; AFNOR NF C 27210
 >= 1e+05
@Temperature 23.0 °C
 >= 1.10e+14 ohm-cm
@Temperature 100 °C
 >= 8.10e+14 ohm-cm
@Temperature 75.0 °C
Dielectric Constant 2.68+5% of mineral oil; AFNOR NF C 27210
 2.7+2% of mineral oil; AFNOR NF C 27210
 2.5
@Temperature 100 °C
50/60 Hz
 2.6
@Temperature 75.0 °C
50/60 Hz
 2.7
@Temperature 23.0 °C
50/60 Hz
Dissipation Factor 0.000061+2% of mineral oil; AFNOR NF C 27210
 0.000075+5% of mineral oil; AFNOR NF C 27210
 0.000031
@Temperature 23.0 °C
50/60 Hz
 0.000031
@Temperature 100 °C
50/60 Hz
 0.000051
@Temperature 75.0 °C
50/60 Hz
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.525 J/g-°C
Thermal Conductivity 0.150 W/m-K
Melting Point -50.0 °C
Flash Point 216 °C+5% of mineral oil, open cup; AFNOR NF T 60118
 247 °C+2% of mineral oil, open cup; AFNOR NF T 60118
 280 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.402
 
Descriptive Properties
AppearanceClear liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Wacker® AK 1000 Silicone Fluid
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 5 Polydimethylsiloxanic Fluids
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2
2-Butanol (CH3CH2CH(OH)CH3; secondary-Butyl Alcohol)

PBLUST107 / 191083

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.