MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ascend Performance Materials HiDura™ MED AG33 NT0862 PA66-GF33
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: HiDura MED AG33 NT is an injection moldable glass fiber reinforced PA66 resin designed for healthcare applications. It is characterized by excellent strength & stiffness for structural needs. The product is compliant to ISO 10993-5 and ISO 10993-10. It is very easy to color and exhibits good property retention after most sterilization methods.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccDAM; ISO 1183
Water Absorption 0.80 %
@Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.7 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 145 MPa50% RH; ISO 527-2
 205 MPaDAM; ISO 527-2
Elongation at Break 3.0 %DAM; ISO 527-2
 5.0 %50% RH; ISO 527-2
Tensile Modulus 7900 MPa50% RH; ISO 527-2
 10600 MPaDAM; ISO 527-2
Flexural Strength 200 MPa50% RH; ISO 178
 290 MPaDAM; ISO 178
Flexural Modulus 6500 MPa50% RH; ISO 178
 10200 MPaDAM; ISO 178
Poissons Ratio 0.40ISO 527-2
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 11.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 12.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 16.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 69.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 71.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 75.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 77.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 86.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 11.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 11.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 11.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 13.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 17.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 106 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 260 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 250 °CUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 310 °CInjection
Middle Barrel Temperature 280 - 310 °CInjection
Front Barrel Temperature 280 - 310 °CInjection
Nozzle Temperature 280 - 310 °CInjection
Melt Temperature 285 - 305 °CInjection
Mold Temperature 65.0 - 95.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
 
Descriptive Properties
AdditiveLubricant
 Release agent
Agency RatingsBSE/TSE Compliant
AppearanceNatural Color
FeaturesBromine Free
 Chemical Resistant
 Corrosion Resistant
 Creep Resistant
 Fatigue Resistant
 Good Colorability
 Good Dimensional Stability
 Good Flow
 Good Impact Strength
 Good Mold Release
 Good Processability
 Good Stiffness
 Halogen Content, None
 High Rigidity
 High Strength
 High Tensile Strength
 Homopolymer
 Hydrolysis Resistant
 Lubricated
 Solvent Resistant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE8503 / 296318

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.