MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Diamond Centrex® 601 Profile Extrusion Grade AES  (discontinued **)
Categories: Polymer; Thermoplastic; AES Polymer; AES, Extruded

Material Notes: Centrex 601 resin is a very high-impact, low-gloss AES (acrylonitrile-ethylene-propylene-styrene) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can be coextruded over polyvinyl chloride (PVC).

Applications: Typical applications for Centrex 601 resin include exterior siding and window frames panels. As with any product, use of Centrex 601 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Weatherable Polymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccASTM D792
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 23.4 MPachs 2.0 in/min; ASTM D638
Tensile Strength, Yield 28.3 MPachs 2.0 in/min; ASTM D638
Tensile Modulus 1722 MPachs 2.0 in/min; ASTM D638
Flexural Strength 44.1 MPachs 0.05 in/min; ASTM D790
Flexural Modulus 1585 MPatangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 80.0 J/m
@Thickness 3.17 mm,
Temperature -40.0 °C
ASTM D256
 128 J/m
@Thickness 3.17 mm,
Temperature -18.0 °C
ASTM D256
 534 J/m
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D256
Impact Test 26.0 J
@Temperature -40.0 °C
ASTM D3763
 38.0 J
@Temperature 23.0 °C
ASTM D3763
 41.0 J
@Temperature -18.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 28.0 µm/m-°CASTM D696
 
Optical PropertiesOriginal ValueComments
Gloss 50 - 70 %Sheet/Profile; 60°; ASTM D523

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for ASA/AES, Unreinforced, Extruded/Molded
Sax Polymers SAXATEC 6120 AES
A. Schulman Diamond Centrex® 813 General Purpose Injection Molding Grade ASA/AES
Mocom (ALBIS) ALTECH® ABS+PMMA A 1000/500 ABS+PMMA
Polyram RamShine PVS701 AES, UV Stabilized

PDIAM351 / 126442

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.