MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
HB Fuller 4189-3 Energy Absorbing Sound Damping Pad
Categories: Other Engineering Material

Material Notes: 4189-3 sound damping pad is a combination of energy absorbing mastic material and an aluminum top layer that provides maximum sound damping. Extension and compression of the mastic damping material converts vibratory energy into heat, thus reducing the noise level of the damped substrate. The aluminum top layer maximizes this effect by redirecting any escaping vibratory energy back into the mastic layer.

Features and Benefits:

  • Adheres to polar and non-polar surfaces.
  • Good Low Temperature Flexibility
  • Can be used on most clean dry substrates
  • Broad application temperature range
  • Reduces noise created by vibration

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.60 g/ccASTM D71
Storage Temperature 10.0 - 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Penetration 90
@Load 0.150 kg
Cone, [dmm]; ASTM D217
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
ColorBlack
ConsistencyFoil-Backed Patch

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL068 / 316859

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.