System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Wieland Eco E4 Casting Alloy
Categories:
Metal
;
Nonferrous Metal
;
Precious Metal
;
Palladium Alloy
;
Silver Alloy
Material Notes:
Silver-palladium casting alloy
Applications: crowns, short span bridges, long span bridges
Dental
Key Words:
EN ISO 8891
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
10.9
g/cc
Mechanical Properties
Original Value
Comments
Hardness, Vickers
130
HV5/30; as cast
130
HV5/30; hardened
Tensile Strength, Yield
37700
psi
@Strain 0.2 %
as cast
37700
psi
@Strain 0.2 %
hardened
Elongation at Break
9.0 %
as cast
9.0 %
hardened
Modulus of Elasticity
96.0
GPa
Thermal Properties
Original Value
Comments
Melting Point
1830
-
1940
°F
Solidus
1830
°F
Liquidus
1940
°F
Processing Properties
Original Value
Comments
Processing Temperature
1290
°F
Preheating Temp.
Casting Temperature
2210
°F
Component Elements Properties
Original Value
Comments
Copper, Cu
4.0 %
Gold, Au
5.0 %
Palladium, Pd
25 %
Silver, Ag
63.5 %
Zinc, Zn
2.5 %
Descriptive Properties
Color
white
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
HGC-4 Precious dental alloy
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Gold, Au; 18K, Yellow (UNS P00255)
Indium Corp. Indalloy 215 Silver Solder Alloy
Lucas-Milhaupt Cerametil 716 Active Metal Brazing
NWIELAN27 / 19829
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.