MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group QGel 319 Optically Clear Silicone Gel
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QGel 319 is an optically clear, moderately cross-linked silicone potting compound. Silicone potting compounds are used to provide protection from vibration and thermal or mechanical shock.

Key Features:

  • 10:1 mix ratio
  • 24 hour room temperature cure
  • Soft, but has considerably higher strength than general purpose silicone gels
  • Dispensing equipment not necessary

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/ccUncatalyzed A
 0.970 g/ccUncatalyzed B
Viscosity 900 cPUncatalyzed A
 3200 cPUncatalyzed B
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 20Cured 30 min. at 150°C
Tensile Strength 0.414 MPaCured
Elongation at Break 120 %Cured
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 20.0 hour
 30.0 min
@Temperature 150 °C
 60.0 min
@Temperature 100 °C
Gel Time 120 minCatalyzed
 
Descriptive Properties
ColorTransparentUncatalyzed A
 TransparentUncatalyzed B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group QGel 311 QSI Quantum Silicones General Purpose Silicone Gel
CHT Group QGel 311 UV Special Purpose Silicone Gel
CHT Group QGel 314 General Purpose Silicone Gel
CHT Group QGel 315 QSI Quantum Silicones General Purpose Silicone Gel
CHT Group QGel 322 General Purpose Silicone Gel

PACC2019 / 199407

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.