MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Primex Plastics Prime ABS Weather-X 200 Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Prime ABS Weather-X 200 is an acrylic capped co-extruded ABS sheet, which can be produced as a two or three multilayer composite. The acrylic cap imparts a very high gloss, vibrant colors with superior depth of image, excellent UV protection, chemical resistance, toughness and excellent formability.

Applications: The performance features of Prime ABS Weather-X 200 make it The material of choice for applications, including marine, personal watercraft, recreational vehicles, lawn/garden, building/construction and automotive accessories.

Information provided by Primex Plastics Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 in/in
 0.0040 - 0.0080 in/inProcessing
Melt Flow 8.9 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 5220 psiASTM D638
Elongation, Ultimate 22 %ASTM D638
Flexural Modulus 280000 psiASTM D790
Izod Impact, Notched 4.40 ft-lb/in
@Thickness 3.17 mm,
Temperature 0.000 °C
ASTM D785
 5.60 ft-lb/in
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 208 °FAnnealed; ASTM D648
 
Optical PropertiesOriginal ValueComments
Gloss 87 %60° Angle; ASTM D523
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 °FDe-mold
 325 - 360 °FSurface Temperature
Mold Temperature 150 - 175 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRIM004 / 278475

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.