Temper: Soft Anneal Fabrication Properties: Excellent Suitability – Soldering, Seam Weld, Butt Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Spot Weld; Fair Suitability – Brazing, Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding Typical uses: Electrical Connectors; Electrical Pinions; Electronic Contacts |