MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Avient Dynaflex™ G2745 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat Aging

Color concentrates with polypropylene (PP), ethylene vinyl acetate (EVA), or polyethylene (PE) carrier are most suitable for coloring Dynaflex™ G2745. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 25 - 40 g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Liquid color can be used, but mineral oil based carriers may have a significant effect on the final hardness value. Concentrates based on PVC should not be used. A high color match consistency can be obtained by using precolored compounds available from GLS. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Regrind levels up to 20% can be used with Dynaflex™ G2745 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt temperature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Dynaflex™ G2745 has excellent melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 0.5 to 3 in/sec 1st Stage - Boost Pressure: 400 to 900 psi

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.888 g/ccASTM D792
Viscosity 9900 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
ASTM D3835
 35000 cP
@Shear Rate 1340 1/s,
Temperature 200 °C
ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 4210 sec; ASTM D2240
Tensile Strength at Break 5.10 MPa
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Tensile Stress at Strain 2.76 MPa
@Strain 300 %,
Temperature 23.0 °C
Die C2 hr; ASTM D412
Elongation at Break 600 %
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Tear Strength 27.3 kN/m
@Temperature 23.0 °C,
Time 7200 sec
ASTM D624
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 196 - 204 °C
Front Barrel Temperature 204 - 216 °C
Nozzle Temperature 216 - 232 °C
Mold Temperature 23.9 - 65.6 °C
Back Pressure 0.000 - 0.552 MPa
 
Compliance PropertiesOriginal ValueComments
FDA Yes21 CFR 177.1210
 
Descriptive Properties
Agency RatingsBfR XXI, section 2.1.3.1.1
AppearanceClear/Transparent
FeaturesGood Colorability
 Good Heat Aging Resistance
 Good Processability
 Ozone Resistant
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAsia Pacific
RoHS ComplianceRoHS Compliant
Suggested Max Regrind20%
UsesConsumer Applications
 Overmolding
 Personal Care
 Soft Touch Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Dynaflex™ G2730 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G2712-1000-02 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G6703-0001 Thermoplastic Elastomer (TPE)

PH0POL1180 / 145749

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.