MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reliance Industries 67-01 Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: Information provided by Reliance Industries

Applications:
Recommended:

  • Rigid extrusion.

    Can be used:

  • rigid injection.
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Bulk Density 0.510 - 0.600 g/ccPVCH/QCD/3516
    Particle Mesh Size 40 MeshTraces; PVCH/QCD/3514
     60 Mesh10% Retention; PVCH/QCD/3514
     140 Mesh25% Retention; PVCH/QCD/3514
    Collected Volatile Condensable Material <= 0.00020 %PVCH/QCD/3520
     
    Descriptive Properties
    Fish Eye count, No. 20PVCH/QCD/3518
    Heat Loss, %(max.)0.3PVCHQCD/3513
    K-Value67PVCH/QCD/3512; 1% in cyclohexanone at 30°C
    Porosity DOP Absorption, ml/g0.21-.029PVCH/QCD/3515

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Reliance Industries 57-01 Polyvinyl Chloride

    PREL087 / 65427

    Master Bond adhesives

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.