MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestamid® L2140 sw 9.7504 (as-conditioned) Nylon 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Extrusion/Tubing Grade

Material Notes: Uses: Tubing for the automobile industry according to DIN 73 378, Type: PA 12-HL.

ISO data as provided by the manufacturer.

Key Words: Polyamide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/cc
Moisture Absorption at Equilibrium <= 0.50 %Humidity Absorption
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 41.0 MPa
Elongation at Break >= 50 %
Elongation at Yield 13 %
Modulus of Elasticity 1.30 GPa
Charpy Impact Unnotched NB
 NB
@Temperature -30.0 °C
Charpy Impact, Notched 1.20 J/cm²
 1.00 J/cm²
@Temperature -30.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 3.00e+14 ohm-cm
Surface Resistance >= 1.00e+15 ohm
Dielectric Constant 3.0
@Frequency 1e+6 Hz
 4.0
@Frequency 100 Hz
Dielectric Strength 35.0 kV/mm
Dissipation Factor 0.050
@Frequency 1e+6 Hz
 0.070
@Frequency 100 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear <= 50.0 µm/m-°C
@Temperature 20.0 °C
Vicat Softening Point 140 °C50°C/hr/50 N
UL RTI, Electrical 120 °C
UL RTI, Mechanical with Impact 85.0 °C
UL RTI, Mechanical without Impact 95.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestamid® L2121 sw 9.7507 (dry properties) Nylon 12
Evonik Vestamid® L2123 Plasticized Nylon 12
Evonik Vestamid® L2140 sw 9.7504 (dry properties) Nylon 12
Evonik Vestamid® L2140 Black Nylon 12 for Fiber Optic Jacketing
Evonik Vestamid® L2121 sw 9.7507 (as-conditioned) Nylon 12

PHUL84 / 47344

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.